Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NIZHNEKAMSKNEFTEKHIM PE 6250D (506H4) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 6250D (506H4) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.948 - 0.952 g/cc
0.0342 - 0.0344 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.30 - 0.50 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 - 0.50 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
5.4 - 9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.4 - 9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.20 GPa
>= 174 ksi
ASTM D790
Izod Impact, Notched >= NB

@Temperature 23.0 °C
>= NB

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: