Material Notes:
Petromont HDPE 5001 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boards, panels, etc.Petromont HDPE 5001 is a high molecular weight hexene modified resin with a broad molecular weight distribution offering an excellent combination of rigidity, toughness and extrusion characteristics.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 2000 hour
>= 2000 hour
F<sub>50</sub>; ASTM D1693-B
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693-B
Melt Flow 0.10 g/10 min
0.10 g/10 min
I<sub>2</sub>; ASTM D1238
11 g/10 min
11 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.1 MPa
5090 psi
ASTM D638
Tensile Strength, Yield 35.1 MPa
5090 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched >= 2.13 J/cm
>= 3.99 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Sheet Extrusion