Axion Polymers Axpoly® HDPE21 1000 High Purity Molding

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Axion Polymers
Trade Name Axpoly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axion Polymers Axpoly® HDPE21 1000 High Purity Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin resinHuge savings in CO2 impactAppeals to 'greener' customersCost-down on raw materialInformation provided by Axion Recycling
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
Particle Size 3000 µm
3000 µm
Pellet Size
Melt Index of Compound 0.18 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.18 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
Elongation at Break 37 %
37 %
Izod Impact, Unnotched (ISO) 83.0 kJ/m²
39.5 ft-lb/in²
Descriptive Properties Value Comments
Visual Appearance Natural