Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0343 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6348K (486F3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6348M (486F8) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.928 - 0.950 g/cc
0.0335 - 0.0343 lb/in³
Average value: 0.938 g/cc Grade Count:30
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Density 0.942 - 0.949 g/cc
0.0340 - 0.0343 lb/in³
Average value: 0.946 g/cc Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..
Density 0.950 - 0.950 g/cc

@Temperature 285 - 285 °C
0.0343 - 0.0343 lb/in³

@Temperature 545 - 545 °F
Average value: 0.950 g/cc Grade Count:1
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Density 0.943 - 0.949 g/cc
0.0341 - 0.0343 lb/in³
Kazanorgsintez 293-285 High Density Polyethylene Composite, Film Grade
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are ..
Density 0.943 - 0.949 g/cc
0.0341 - 0.0343 lb/in³
Kazanorgsintez 293-285D High Density Polyethylene Composite, Film Grade
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are ..
Density 0.943 - 0.949 g/cc
0.0341 - 0.0343 lb/in³
Kazanorgsintez 297-285 High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-..
Density 0.943 - 0.949 g/cc
0.0341 - 0.0343 lb/in³
Kazanorgsintez 297-285D High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-..
Density 0.944 - 0.950 g/cc
0.0341 - 0.0343 lb/in³
ASTM D792-98
Ipiranga Petrochem HD 7555 LS-L HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Density 0.925 - 0.950 g/cc
0.0334 - 0.0343 lb/in³
ASTM D1505
Micropol Microlink XL Crosslinkable Polyethylene
Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi..
Density 0.943 - 0.949 g/cc
0.0341 - 0.0343 lb/in³
Kazanorgsintez 293-285SK High Density Polyethylene Composite, Film Grade
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are ..
Density 0.945 - 0.949 g/cc
0.0341 - 0.0343 lb/in³
ASTM D792-98
Ipiranga Petrochem GM 7040 G HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Density 0.940 - 0.950 g/cc
0.0340 - 0.0343 lb/in³
Solvay CATAFOR® CA80 Surfactant
Identification: QUATERNARY AMMONIUM ETHOSULPHATECAS: 68308 – 64 – 5Solubility: Readily soluble in ethyl alcohol, butanol chloroform, trichloroethylene, ethyl acetate and water.Solvent: n-B..
Density 0.910 - 0.950 g/cc
0.0329 - 0.0343 lb/in³
ISO 1183
Fainplast Compounds Hax™ CAT 100T Catalyst for Cable Compound
Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Low reactive catalystInformation provided by Fainplast Compounds
Density 0.910 - 0.950 g/cc
0.0329 - 0.0343 lb/in³
ISO 1183
Fainplast Compounds Hax™ CAT 103T Catalyst for Cable Compound
Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• High reactive cataylstInformation provided by Fainplast Compounds
Density 0.910 - 0.950 g/cc
0.0329 - 0.0343 lb/in³
ISO 1183
Fainplast Compounds Hax™ CAT 111 Catalyst for Cable Compound
Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Cataylst for extreme ageing conditionsInformation provided by Fainplast Compounds
Density 0.910 - 0.950 g/cc
0.0329 - 0.0343 lb/in³
ISO 1183
Fainplast Compounds Hax™ CAT 113 Catalyst for Cable Compound
Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Cataylst for extreme ageing conditionsInformation provided by Fainplast Compounds
Density 0.910 - 0.950 g/cc
0.0329 - 0.0343 lb/in³
ISO 1183
Fainplast Compounds Hax™ CAT 115/1 Catalyst for Cable Compound
Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• High reactive cataylstInformation provided by Fainplast Compounds
Density 0.910 - 0.950 g/cc
0.0329 - 0.0343 lb/in³
ISO 1183
Fainplast Compounds Hax™ CAT 115LS Catalyst for Cable Compound
Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Low reactive catalystInformation provided by Fainplast Compounds
Density 0.940 - 0.950 g/cc
0.0340 - 0.0343 lb/in³
Average value: 0.941 g/cc Grade Count:27
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Density 0.900 - 0.950 g/cc
0.0325 - 0.0343 lb/in³
DIN 52004
Lucobit Lucosol® Bitumen Road Binder
Lucosol is a solvent based bitumen road binder made out of selected bitumen qualities and hydrocarbon solventsInformation provided by Lucobit AG
Copyright © lookpolymers.com All Rights Reserved