Borealis BorPEX™ HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Borealis
Trade Name BorPEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPEX™ HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorPEX HE2590 is a high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization is optimized for good processability, easy crosslinking as well as service at high temperatures.Crosslinked pipes based on BorPEX HE2590 are recommended for domestic hot and cold water supply, natural gas distribution, radiator connection, floor heating and industrial applications.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
Base Resin; ISO 1183
0.946 g/cc
0.0342 lb/in³
Compound; ISO 1183
High Load Melt Index 8.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.00 MPa
2611 psi
At 50 mm/min; ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2