| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycolac® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
| Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 5.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| 18 g/10 min @Load 10.0 kg, Temperature 220 °C |
18 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 112 | 112 | ASTM D785 |
| Tensile Strength at Break | 33.0 MPa | 4790 psi | Type I, 5 mm/min; ASTM D638 |
| 35.0 MPa | 5080 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 44.0 MPa | 6380 psi | Type I, 5 mm/min; ASTM D638 |
| 47.0 MPa | 6820 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 24 % | 24 % | Type I, 5 mm/min; ASTM D638 |
| 25 % | 25 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 2.0 % | 2.0 % | Type I, 5 mm/min; ASTM D638 |
| 2.5 % | 2.5 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
| 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 70.0 MPa | 10200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 70.0 MPa | 10200 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
| 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
| Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
| 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 2.60 J/cm² | 12.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 98.0 °C | 208 °F | Rate B/50; ISO 306 |
| 99.0 °C | 210 °F | Rate B/50; ASTM D1525 | |
| 100 °C | 212 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
| UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |