Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 18 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 220 °C
18 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East)
CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona..
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG47 ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
Melt Flow 18 g/10 min

@Load 1.00 kg,
Temperature 235 °C
18 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
Network Polymers Softflex® 0921
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 220 °C
18 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East)
Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® EXRL0682 PC Copolymer
18 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Melt Flow 18 - 24 g/10 min

@Load 21.6 kg,
Temperature 190 °C
18 - 24 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4222M (224F7) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Iran Petrochemical (PCC) 5218EA High Density Polyethylene
HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed..
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 230 °C
18 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800R PC
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics PC1803R PC
PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was..
Melt Flow 18 - 24 g/10 min

@Load 5.00 kg,
Temperature 230 °C
18 - 24 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF)
Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 265 °C
18 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 260 °C
18 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics NORYL N850 PPE+PS
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 260 °C
18 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific)
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 250 °C
18 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 240 °C
18 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ASTM D 1238
Cossa Polimeri ESTADIENE 1218 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, high thermal resistanceInformation provided by Cossa Po..
Melt Flow 18 g/10 min

@Load 21.6 kg,
Temperature 220 °C
18 g/10 min

@Load 47.6 lb,
Temperature 428 °F
ASTM D 1238
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Melt Flow 18 - 24 g/10 min

@Load 5.00 kg,
Temperature 230 °C
18 - 24 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers.
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Polimeri Europa SINKRAL G523 ABS, High Impact  (discontinued **)
High impact; good flow; high gloss.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 230 °C
18 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238 (I)
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 260 °C
18 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics GELOY XP4025 ASA+PC
Available in a wide range of colors and is recommended for unpainted exterior applications.
Copyright © lookpolymers.com All Rights Reserved