Polymer Property : Vicat Softening Point = 208 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
SABIC 218 Series Linear Low Density Polyethylene for Blown Film
Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a..
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
Vicat Softening Point 98.0 °C
208 °F
Rate A/50; ISO 306
SABIC Innovative Plastics Cycolac® MG8000SR ABS
This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 98.0 °C
208 °F
Rate A/50; ISO 306
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific)
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific)
CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla..
Vicat Softening Point 98.0 °C
208 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications.
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific)
PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific)
BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance ..
Vicat Softening Point 98.0 °C
208 °F
Americas Styrenics Styron® 6187SF High Impact Polystyrene  (discontinued **)
STYRON® 6187SF structural foam molding resin is a high impact polystyrene grade with proprietary ignition resistance additive package to achieve UL 94 V-0 rating. It offers excellent moldability an..
Vicat Softening Point 98.0 °C
208 °F
50N (T° increase = 5°C/h); ISO 306B50
Total Lacqrene® 1250 Crystal Polystyrene  (discontinued **)
LACQRENE® 1250 is a very high molecular weight crystal polystyrene mainly for the injection molding industry. It is characterized by a very good compromise between molecular weight, heat resistanc..
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Huntsman PE1031 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund..
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Braskem PB 526 LDPE Blow Molding Polyethylene  (discontinued **)
Applications: Heavy duty bags; tubes and hoses; shrink films for pallets; tarpaulins. Blown Film. Information provided by Braskem
Vicat Softening Point 98.0 °C
208 °F
1 kg; ASTM D1525
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding
Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha..
Vicat Softening Point 97.8 °C
208 °F
50°C/h 50N
Ineos ABS Lustran® PG 298
Key Features:UnfilledPlatableSuitable processing methods:Injection molding
Vicat Softening Point 98.0 °C
208 °F
ISO 306A
Lucite International Diakon® CLG960 Acrylic Polymer
Information provided by Lucite International
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
KKPC Kuhmo MIB 237 Blow Molding HIPS
Key features: Good-profiling, Thin-layer Molding. Common Uses: It is used exclusively as a container for fermented milk beverages.HIPS is a functional resin made by copolymerization of styrene monom..
Vicat Softening Point 98.0 °C

@Load 5.00 kg
208 °F

@Load 11.0 lb
50°C/h; ASTM D1525
LG Chemical MA221 ABS, High Impact, Low Gloss
Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Vicat Softening Point 98.0 °C
208 °F
B/50; ISO R306
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 98.0 °C

@Load 5.10 kg
208 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution Absolac® 200 ABS
Electroplating gradeInformation provided by Styrolution
Vicat Softening Point 98.0 °C
208 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS
high gloss Noryl
Vicat Softening Point 98.0 °C
208 °F
ISO 306
Total FE 8000 LDPE blown film
Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired form..
Vicat Softening Point 98.0 °C

@Load 1.02 kg
208 °F

@Load 2.25 lb
50°C per hour; ASTM D1525
Total PSC 1441 Easy Flow, High Heat Resistance Polystyrene
Total Petrochemicals Polystyrene 1441 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle time..
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Dow DOWLEX™ 2047G Linear Low Density Polyethylene
For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Huntsman PE2065 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: General purpose injection molding resin with good flow characteristicsApplications: Injection molding: lids.FDA Notes: Conforms to FDA regulation 21 CFR 177.1..
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Huntsman PE2067 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: High flow resin, provides excellent gloss and surface characteristics, and minimum cycle time.Applications: Injection molding: lids.FDA Notes: Conforms to FDA..
Vicat Softening Point 97.8 °C
208 °F
ASTM D1525
Total PSI 975E Polystyrene
Polystyrene 975E is a high impact polystyrene designed for extrusion/thermoforming applications. The food ESCR properties of 975E dictate its use for dairy applications that are subjected to high bu..
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Cycoloy® CY4000M PC+ABS (Asia Pacific)
Cycoloy* CY4000M resin is an injection moldable, flame retardant PC/ABS blend free of chlorinated or brominated flame resistant additives. Cycoloy CY4000M resin has excellent flow and balanced impac..