| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648-56 |
| Rotuba 890 Ethyl Cellulose Data provided by the manufacturer. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
| SABIC PP 5702P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| SABIC Innovative Plastics Cycolac® EX75 ABS Multi-purpose, extrusion ABS providing a favorable balance of engineering properties. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| SABIC Innovative Plastics Cycolac® INPBMAT ABS Cross-linked SAN in styrenic matrix. Provides excellent gloss reduction properties. Maintains original polymer properties such as impact etc. Compatible with various polymer such as PVC and ABS. C.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| SABIC Innovative Plastics Cycolac® MG47N ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
| LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | |
| Ineos ABS Lustran® PG 298 Key Features:UnfilledPlatableSuitable processing methods:Injection molding |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ISO 75-1,-2 |
| Ineos ABS Lustran® ABS 970 Lustran® ABS 970 has high impact strength and good paintability. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
| LyondellBasell Astryn BA66K Polypropylene Copolymer, Flame Retardant Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, high limiting oxygen index, non-halogenated, good aesthetics, excellent processabilityApplications: batteries, .. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
| Techmer ES HiFill FR® ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantTPCI# 1039121Information provided by TP Composites, Inc. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ISO 75 |
| Teijin Multilon TN-7000 Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It is a typical type with high flowability, light resistance and heat stability that is suitable for a business machine .. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Unannealed; ISO 75-2/B |
| Samsung Cheil Industries Infino® PCA-NH1015V Flame Retardant |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
ASTM D648 |
| Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | unannealed; ISO 75-B |
| Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Unannealed; ASTM Data |
| Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Unannealed; ASTM Data |
| Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
| Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
| Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
| Aclo Accutech ABS ABS831G10L Glass Reinforced |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
| Braskem H 306 Fiber Extrusion Polypropylene Applications: Staple fibers for carpets and blankets. Information provided by Braskem |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
| Carmel Olefins CAPILENE® E 50 E Polypropylene Homopolymer CAPILENE® E 50 E is a low melt flow rate polypropylene homopolymer intended for extrusion, thermoforming and blow molding featuring very good process ability and melt stability. Products manufactur.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
| Carmel Olefins CAPILENE® E 65 F Polypropylene Homopolymer Description: CAPILENE® E 65 F is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It exhibits good processability, easy film stretchabilit.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 6.35 mm |
201 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Covestro Bayblend® SF 1443 Polycarbonate + ABS Blend Structural Foam
(discontinued **) Foam thickness 0.250 in. Properties values at foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from .. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | |
| Ineos ABS Centrex® HGM ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | |
| Polimeri Europa KOBLEND PCA 51 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 90°C Main application field.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | |
| Polimeri Europa SINKRAL G323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-20 General purpose injection moulding grade. Main properties are: good impact resistance high flow e.. |
|||