| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® MG37CR ABS High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East) CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties for a wide variety of applications including business equipment, TVs, monitors, enclosures, among others.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
| UL RTI, Electrical | 60.0 °C @Thickness 1.60 mm |
140 °F @Thickness 0.0630 in |
UL746B |
| Ineos ABS Lustran® 1148 General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
| UL RTI, Electrical | 60.0 °C @Thickness 1.60 mm |
140 °F @Thickness 0.0630 in |
UL746B |
| Ineos ABS Lustran® Ultra 2337 General Purpose, Superhigh-Gloss
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | Average value: 60.0 °C Grade Count:10 |
| Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
| UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL746B |
| Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
| UL RTI, Electrical | 60.0 °C @Thickness >=1.70 mm |
140 °F @Thickness >=0.0669 in |
|
| LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
| UL RTI, Electrical | 60.0 °C @Thickness >=1.70 mm |
140 °F @Thickness >=0.0669 in |
|
| LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
| UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL746B |
| Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Dry as Extruded Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
| UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
|
| Covestro Bayblend® FR 86 Polycarbonate/ABS Blend Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | |
| Covestro Bayblend® T 45 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| SABIC Innovative Plastics Cycoloy® C1100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100 is a PC+ABS blend developed to satisfy the demanding application requirements, where optimum combination is needed of superior processing efficiency, excellent ductility also at sub ze.. |
|||
| UL RTI, Electrical | 60.0 - 80.0 °C | 140 - 176 °F | Average value: 63.3 °C Grade Count:4 |
| Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||