| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® FR15U ABS (Europe-Africa-Middle East)
CYCOLAC FR15U is a flame retardant ABS with good processability and good indoor UV properties.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® MG38N ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)>
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® MGABS01 ABS
Injection molding ABS. High impact, high gloss, good flow.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East)
CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East)
Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact proper..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® EHA PC+ABS (Asia Pacific)
PC+ABS. Electroplateable.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS
Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific)
PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
|
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific)
Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
|
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo..
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness 1.60 mm |
140
°F @Thickness 0.0630 in |
UL746B |
|
Ineos ABS Lustran® 1148 General Purpose, High-Impact
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness 1.60 mm |
140
°F @Thickness 0.0630 in |
UL746B |
|
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **)
A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va..
|
|||
| UL RTI, Mechanical with Impact | 60.0 - 65.0 °C | 140 - 149 °F | Average value: 61.7 °C Grade Count:6 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness 1.50 mm |
140
°F @Thickness 0.0591 in |
UL746B |
|
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness 1.50 mm |
140
°F @Thickness 0.0591 in |
|
|
Covestro Bayblend® T 64 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| UL RTI, Mechanical with Impact |
60.0
°C @Thickness 1.50 mm |
140
°F @Thickness 0.0591 in |
|
|
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,..
|
|||
| UL RTI, Mechanical with Impact | 60.0 - 80.0 °C | 140 - 176 °F | Average value: 63.3 °C Grade Count:4 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
|
|||