| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPH TS15020 D Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE
Information provided by Polykemi AB
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Total Lacqrene® 1235 High Impact Polystyrene
(discontinued **)
LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of ..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Ineos Styrenics 166H General Purpose Polystyrene (NAFTA)
Description: Polystyrene 166H is a high molecular weight general purpose polystyrene with good flow and crystal clarity. Polystyrene 166H offers good processing characteristics while yielding parts ..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
KKPC Kuhmo HI 425 E Extrusion Molding HIPS
Key features: Cold-resistant Extrusion. Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin ..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
KKPC Kuhmo HI 425TVG High Flow/High Heat Resistant HIPS
Key features: High-impact, High-fluidity Common Uses: TV cover (gas injection).HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between im..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Ineos ABS Lustran® ABS 650 Injection Molding Grade
Lustran® ABS 650 has high impact strength, high flow, and is injection molding grade.
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Ineos ABS Lustran® ABS 970
Lustran® ABS 970 has high impact strength and good paintability.
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics LNP Lubricomp FFL21 PE (Asia Pacific)
LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Styrolution PS 153F GPPS
Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Styrolution PS 156F GPPS
Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Styrolution PS 485N HIPS
Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D 792 |
|
Styrolution PS 5410 HIPS
Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM Data |
|
Styron Magnumâ„¢ 341 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSR65T20 is a 20% mineral filled grade for injection molding. Daplen KSR65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSR65T20 offers very g..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO R1183 |
|
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Aclo Accutech Polypropylene Copolymer CP0436W20L1 Wollastonite Reinforced |
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Buckeye Polymers BP ABS 4332 ABS
Low GlossABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Ashley Polymers Ashlene® ABS Resin F-216
General purpose high impact resin.Data provided by the manufacturer
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
A.D. Compound Adene NCFA Homopolymer 20% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | |
|
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Buckeye Polymers BP ABS 4233 B ABS
Utility GradeABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proces..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
|
Total Lacqrene® 740 High Impact Polystyrene
(discontinued **)
LACQRENE® alpha 740 is a high gloss, high impact grade of polystyrene.ApplicationWhite goods (washing machines, driers), Toys and games, Garden equipment, All applications needing high gloss with g..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Ineos Nova 5420 High Impact Polystyrene
(discontinued **)
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Ineos Nova 5500 High Impact Polystyrene
(discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..
|
|||
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
|
Ineos Nova 5190 High Impact Polystyrene
(discontinued **)
Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C ..
|
|||