| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycolac® X11 ABS
Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS
Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
|
SABIC Innovative Plastics Cycoloy® FXC810FE PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810FE is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ferrite colour effects. The colour package may effect performance.This data was supp..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
|
SABIC Innovative Plastics Lexan® 945ASR PC
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
|
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East)
Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific)
Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific)
High impact and ductility at 73F (23C) and -20F (-29C).
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
|
LG Chemical 20HRI GPPS
Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S..
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness 0.750 - 0.820 mm |
15
-
30
sec @Thickness 0.0295 - 0.0323 in |
|
|
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant
Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness >=0.750 mm |
15
-
30
sec @Thickness >=0.0295 in |
|
|
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness >=0.750 mm |
15
-
30
sec @Thickness >=0.0295 in |
|
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
|
LG Chemical 92HR SAN Resin
Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics NORYL PX1543 PPE+PS |
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 451E PBT
20% GR. Easy flow version of VALOX 451.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 451E PBT (Asia Pacific)
20% GR. Easy flow version of VALOX 451.
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness 3.00 mm |
15
-
30
sec @Thickness 0.118 in |
UL Rating PLC 3 (15-30 sec) |
|
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness 3.00 mm |
15
-
30
sec @Thickness 0.118 in |
UL Rating PLC 3 (15-30 sec) |
|
Covestro Bayblend® T 64 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness 3.00 mm |
15
-
30
sec @Thickness 0.118 in |
UL Rating PLC 3 (15-30 sec) |
|
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia..
|
|||
| Hot Wire Ignition, HWI |
15
-
30
sec @Thickness 1.50 mm |
15
-
30
sec @Thickness 0.0591 in |
UL Rating PLC 3 (15-30 sec) |
|
Covestro Makrolon® 2605 Polycarbonate, Injection Grade
Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
|
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS
LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content.
|
|||
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
|
LG Chemical 402 AF Flame Retardant HIPS
NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t..
|
|||