Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 100 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
B
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant
FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin..
Vicat Softening Point 100 °C
212 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycolac® HMG47MD ABS
General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
Vicat Softening Point 100 °C
212 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS (Asia Pacific)
Vicat Softening Point 100 °C
212 °F
10 N - 50°C/h; ISO 306/A
Polimeri Europa Edistir ICE S 800/N Polystyrene  (discontinued **)
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin  (discontinued **)
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design, low temperature impact excellent.Data provided by the manufacturer.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin  (discontinued **)
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Applications: Thin walled container lids and closures.Data provided by the manufacturer.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
M. Holland Company LL800 LLDPE  (discontinued **)
Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low WarpageUses: Containers, Household Goods, Lids, Thin-walled PartsApprovals: FDA 21 CFR 177.1520(c) 3.2a ..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Chevron Phillips 4538B LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 05200Characteristics: Good Flexibility, Moderate Flow, Moderate Warping Resistance, Good Mold Release, Excellent ESCRApplications:Perso..
Vicat Softening Point 100 °C
212 °F
50°C/h 50N
Ineos ABS Centrex® 821 ASA Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection ..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Lucky CF-920 Acrylic
May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Vicat Softening Point 100 °C
<br>@Load 5.00 kg
212 °F
<br>@Load 11.0 lb
50°C/h; ASTM D1525
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Vicat Softening Point 100 °C
<br>@Load 5.00 kg
212 °F
<br>@Load 11.0 lb
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Vicat Softening Point 100 °C
<br>@Load 5.00 kg
212 °F
<br>@Load 11.0 lb
LATI Latistat 36/MR-04 ABS
Dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Vicat Softening Point 100 °C
212 °F
Rate B/120; ISO 306
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
Vicat Softening Point 100 - 102 °C
212 - 216 °F
ISO 306, B50
Samsung Cheil Industries Infino® PCA-NH1015V Flame Retardant
Vicat Softening Point 100 °C
<br>@Temperature 50.0 °C
212 °F
<br>@Temperature 122 °F
ISO 306
Styrolution Terluran® HD-15 ABS
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Vicat Softening Point 100 °C
212 °F
B/120; ISO R306
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced
Anti-staticInformation provided by Samsung Cheil Industries.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin
Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati..
Vicat Softening Point 100 °C
212 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane
Features: Very resilient product with excellent resistance to abrasion and tearing, low temperature flexibility, and resistant to certain chemicals.Uses: Hot melt adhesive, synthetic leather and fab..
Vicat Softening Point 100 °C
212 °F
Loading 1, Rate A; ASTM D1525
Chevron Phillips Marlex® 7104 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRGood melt strengthExcellent flexibilityGood processabilityGood glossHigh COFApplications: Landfill coversFlat and round-die productsCoext..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed..
Vicat Softening Point 100 °C
212 °F
BASF Procom® GC30S 401 Polypropylene
Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Huntsman PE2051 Injection Molding Polyethylene &nbsp;(discontinued **)
Homopolymer and FDA compliant.Features: Very good molding processability, produces parts with good stiffness, and shows excellent flatness in large projected areas. Also recommended for multi-cavit..
Vicat Softening Point 100 °C
212 °F
B
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 100 °C
212 °F
B/50; ISO R306
Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 100 °C
212 °F
1kg / 120°C; ASTM D1525
Supreme Petrochem SP 8001 High Gloss, ESCR High Impact Polystyrene
Characteristics Very high toughness Excellent ESCR properties against common food chemicals High gloss & heat resistance Processing Extrusion & Forming Applications Fatty food containers Co-extru..
Copyright © lookpolymers.com All Rights Reserved