Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 178 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Annealed; ASTM D648
Network Polymers NPS 90-0827 Polystyrene
Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
120°C/h; ASTM D 648
Polimeri Europa Edistir RC 600 Polystyrene
Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
120°C/h; ISO 75/1
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
120°C/h; ASTM D 648
Polimeri Europa Edistir RCL 600 Polystyrene  (discontinued **)
Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow
Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LUMIPLAS LD590T Light diffusion ABS
Description: Extrusion, Light diffusion, High ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 12.7 mm
178 °F

@Thickness 0.500 in
Unannealed; ASTM D648
LG Chemical 60HR HIPS
Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu..
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® ABS FR BK
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® ABS FR UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Spartech Royalstatâ„¢ R671 ABS Static Control Sheet
Data provided by the manufacturer.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 3.20 mm
178 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific)
LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Supreme Petrochem SC 206 General Purpose Polystyrene
CharacteristicsGood flow grade with clarity & shine Improves aesthetics of final product Processing MoldingApplications Crystal ware, paper weights, house ware Beads, Bangles, gift articles, trays,..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Supreme Petrochem SP 243 Toughened Polystyrene
CharacteristicsGood flexibility Good clarity High stiffnessProcessing Extrusion ThermoformingApplications Clear thermoformed containers Oriented PS films LidsMaterial Status: Commercial : ActiveA..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Supreme Petrochem SP 253 Toughened Polystyrene
Characteristics High rigidity Improved toughness Good clarityProcessing Injection moldingApplications Ball pens Small appliances housings Small impellersMaterial Status: Commercial : ActiveAgenc..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene
Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unifo..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ISO 75-2
Borealis MD441U Polypropylene Compound, Mineral Filled
MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
0.25 inch; ASTM D648
PlastxWorld DAICEL STYROL® GH10 HIPS
High heat resistance and flame retarded HIPS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Eastman Tritan TX1500HF Copolyester
Eastman Tritan TX1500HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1500HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1000. Other outstanding features..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
ASTM D648
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Aclo Accutech Polypropylene Homopolymer HP0339M40L Mica Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Ineos Nova 3511 General Purpose Crystal Polystyrene  (discontinued **)
Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 - 216 °C
178 - 421 °F
Average value: 191 °C Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved