Material Notes:
Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applications: Clearflex MQ F0 is suitable for injection molding. Products made with Clearflex MQ F0 are characterized by a high flexibility. Clearflex MQ F0 is recommended for seals and gaskets, for blend with polyolefins to modify and improve impact resistance.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.895 g/cc
0.895 g/cc
ISO 1183
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 26
26
ISO 868/A
Tensile Strength at Break 9.00 MPa
1310 psi
ISO 527
Tensile Strength, Yield 4.00 MPa
580 psi
ISO 527
Elongation at Break 750 %
750 %
ISO 527
Flexural Modulus 0.0450 GPa
6.53 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
Internal method
Vicat Softening Point 51.0 °C

@Load 1.00 kg
124 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified