| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm <br>@Thickness 3.20 mm |
0.0040 - 0.0060 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 20 g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C |
20 g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 113 | 113 | ASTM D785 |
| Tensile Strength, Yield | 58.8 MPa <br>@Thickness 3.20 mm |
8530 psi <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | >= 80 % <br>@Thickness 3.20 mm |
>= 80 % <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 93.2 MPa <br>@Thickness 3.20 mm |
13500 psi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Flexural Modulus | 2.65 GPa <br>@Thickness 3.20 mm |
384 ksi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Izod Impact, Notched | >= 3.43 J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
>= 6.43 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C <br>@Thickness 6.40 mm |
208 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 60.0 °C <br>@Thickness >=1.20 mm |
140 °F <br>@Thickness >=0.0472 in |
|
| 80.0 °C <br>@Thickness >=1.50 mm |
176 °F <br>@Thickness >=0.0591 in |
||
| 80.0 °C <br>@Thickness >=2.00 mm |
176 °F <br>@Thickness >=0.0787 in |
||
| 80.0 °C <br>@Thickness >=2.50 mm |
176 °F <br>@Thickness >=0.0984 in |
||
| 80.0 °C <br>@Thickness >=3.00 mm |
176 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 60.0 °C <br>@Thickness >=1.20 mm |
140 °F <br>@Thickness >=0.0472 in |
|
| 80.0 °C <br>@Thickness >=1.50 mm |
176 °F <br>@Thickness >=0.0591 in |
||
| 80.0 °C <br>@Thickness >=2.00 mm |
176 °F <br>@Thickness >=0.0787 in |
||
| 80.0 °C <br>@Thickness >=2.50 mm |
176 °F <br>@Thickness >=0.0984 in |
||
| 80.0 °C <br>@Thickness >=3.00 mm |
176 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 60.0 °C <br>@Thickness >=1.20 mm |
140 °F <br>@Thickness >=0.0472 in |
|
| 85.0 °C <br>@Thickness >=1.50 mm |
185 °F <br>@Thickness >=0.0591 in |
||
| 85.0 °C <br>@Thickness >=2.00 mm |
185 °F <br>@Thickness >=0.0787 in |
||
| 85.0 °C <br>@Thickness >=2.50 mm |
185 °F <br>@Thickness >=0.0984 in |
||
| 85.0 °C <br>@Thickness >=3.00 mm |
185 °F <br>@Thickness >=0.118 in |
||
| Flammability, UL94 | V-0 <br>@Thickness >=1.20 mm |
V-0 <br>@Thickness >=0.0472 in |
|
| V-0 <br>@Thickness >=1.50 mm |
V-0 <br>@Thickness >=0.0591 in |
||
| V-0 <br>@Thickness >=2.00 mm |
V-0 <br>@Thickness >=0.0787 in |
||
| V-0 <br>@Thickness >=2.50 mm |
V-0 <br>@Thickness >=0.0984 in |
||
| V-0 <br>@Thickness >=3.00 mm |
V-0 <br>@Thickness >=0.118 in |
||
| 5VB <br>@Thickness >=2.50 mm |
5VB <br>@Thickness >=0.0984 in |
||
| 5VB <br>@Thickness >=3.00 mm |
5VB <br>@Thickness >=0.118 in |
||
| 5VA <br>@Thickness >=1.50 mm |
5VA <br>@Thickness >=0.0591 in |
||
| 5VA <br>@Thickness >=2.00 mm |
5VA <br>@Thickness >=0.0787 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | |
| Hot Wire Ignition, HWI | 30 - 60 sec <br>@Thickness >=1.20 mm |
30 - 60 sec <br>@Thickness >=0.0472 in |
|
| 30 - 60 sec <br>@Thickness >=1.50 mm |
30 - 60 sec <br>@Thickness >=0.0591 in |
||
| 30 - 60 sec <br>@Thickness >=2.00 mm |
30 - 60 sec <br>@Thickness >=0.0787 in |
||
| High Amp Arc Ignition, HAI | 30 - 60 arcs <br>@Thickness 1.20 mm |
30 - 60 arcs <br>@Thickness 0.0472 in |
|
| >= 120 arcs <br>@Thickness 1.50 mm |
>= 120 arcs <br>@Thickness 0.0591 in |
||
| >= 120 arcs <br>@Thickness 2.00 mm |
>= 120 arcs <br>@Thickness 0.0787 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
| Middle Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
| Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
| Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
| Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
| Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
| Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
| Back Pressure | 0.0200 - 0.0600 MPa | 2.90 - 8.70 psi | Injection Molding |
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |