Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 161J-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ISO 178, ASTM D790 |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific) Mineral filled Antistatic Polycarbonate, HDT110degC type |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 6.40 mm |
384 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness Feature: Injection Molding, High Transparency, High Rigidity, High HardnessApplication: Electric/Electronic Parts Copier, Compact Cases etc.CAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 201LV General Purpose Polystyrene CharacteristicsHigh molecular weight grade Good flow properties along with good mechanical strength Easy process ability with good mold release propertiesProcessing Injection moldingApplicationsSuit.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 30% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2mm/min; ISO 178 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
E-Polymers TEKAMID® TA210IR Impact Modified PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ISO 178 |
Cathay PA56 Renewable Engineering Polyamide, DAM Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound R7550 CLR 223V is a general purpose medium/high impact profile extrusion compound developed for ease of process, sparkling clarity and gloss. It has been formulated for UV resistance for interior a.. |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | ASTM D790 |
Aaron Industries AVPS M 100-2 Virgin Polystyrene Melt flow index may be specified. |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | ASTM D790 |
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade BRC R7560 CLR 221 is a food grade PVC bottle compound made with 100% FDA approved ingredients. This product exhibits excellent clarity and can be used in many applications where food contact is req.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
Tipco Tipcolene® FPDG-M FPDG M - 28% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CompoundApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |