| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Plastcom PLASTAMID® 6 BT N 32 B/IM PA6
Basic type PA 6 for injection molding, compounding, for general use. Use: automotive, engineering, electrical and consumer goods industry - electrical tools, fasteners, clamps, hobby tools, toys. De..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Plastcom SLOVAMID 66 HI Polyamide 66, Impact Grade
FeaturesModified with thermoplastic reactive elastomer, determined for mouldings with high toughness also at low temperatures. Eligible application for ski-shoes, helmets for sport and other safety..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Plastcom SLOVAMID 66/6 HI/1 PA66/6, improved strength
FeaturesMix of polyamide 66/6 modified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets fo..
|
|||
| Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
|
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
|
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre
Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Premix Thermoplastics PRE-ELEC® PP 1385
PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
PolyOne Bergadur™ PB40 G15 blue Polybutylene Terephthalate (PBT)
Information provided by PolyOne
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | Start Point: 60°C |
|
Kingfa MAC-701 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, Conditioned
Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Teknor Apex Beetle® A82 Nylon 66, Non-Halogenated
Notes: A82 is a UL recognized. V-0 rated halogen and phosphorus-free flame retarded, heat stabilized, unreinforced injection molding grade of nylon 66. Features: Flame Retardant; Heat Stabilized; Ha..
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Zhejiang Juner JEPP263 Weatherability PP Series
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Mold Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Ecomass® 1850ZN66T1 Steel Powder Filled Polyamide, Injection Molding
Steel Powder Filled Polyamide (PA6), Impact Modified, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInformation provide..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing..
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
CP-Polymer-Technik Wellamid® 6000/50 HWUVCP Nylon 6, Impact Modified Until 0°C, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded
AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded
BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded
PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
E-Polymers TEKASTER® F10G30 30% Glass Fiber Reinforced PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
|
|||
| Mold Temperature | 20.0 - 80.0 °C | 68.0 - 176 °F | |
|
Arkema Group Rilsan® Clear G380 Renew Polyamide
Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited..
|
|||
| Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
|
Asahi Kasei Xyron® X9653 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | Injection-molding |
|
BASF Ultramid® B3L BK00464 PA6 (Conditioned)
Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall ..
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Beijing Chemical Industry KAIFA® 301-G10 PBT Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Beijing Chemical Industry KAIFA® GL1100 ABS General Purpose Grade
High gloss, excellent external appearanceInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin
10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss
Information provided by Polykemi AB
|
|||
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | Injection Molding |
|
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN
Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
LATI Latimass 82-05 D040 PA12