Electrical Properties Metric English Comments
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow
Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced
Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced
Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
UL 746
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 0.400 mm
30 - 60 arcs

@Thickness 0.0157 in
PLC 2; UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 0.750 mm
30 - 60 arcs

@Thickness 0.0295 in
PLC 2; UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
BK
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG ..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.20 mm
30 - 60 arcs

@Thickness 0.0472 in
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.20 mm
30 - 60 arcs

@Thickness 0.0472 in
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 0.820 mm
30 - 60 arcs

@Thickness 0.0323 in
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance
Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 0.820 mm
30 - 60 arcs

@Thickness 0.0323 in
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.20 mm
30 - 60 arcs

@Thickness 0.0472 in
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
High Amp Arc Ignition, HAI 30 - 59 arcs

@Thickness 0.400 mm
30 - 59 arcs

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
High Amp Arc Ignition, HAI 30 - 59 arcs

@Thickness 0.400 mm
30 - 59 arcs

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 1.50 mm
30 - 60 arcs

@Thickness 0.0591 in
LG Chemical SG175G ABS, Super Surface Gloss, High Flow
Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved