Polymer Property : Tensile Strength, Yield = 8530 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUCON CP6062EX PC/ABS+CNT
Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, ..
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL GP2150 PP+GF15%
Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® GP1000A PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® GP1000D PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® GP1000S PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5000GU PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info..
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5000S PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided..
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5000SZ PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa
8530 psi
Microcell Composite Company CELLOMER® 6000 SBS Rubber Pellets
CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact
High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact
High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-1051 PC, Unreinforced High Impact
High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-1070 PC, Unreinforced High Impact
High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
ASTM D638
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang
Tensile Strength, Yield 58.8 MPa
8530 psi
ASTM D638
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
Type 1; 5mm/min; ASTM D638
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy
ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact
High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 58.8 MPa
8530 psi
ASTM D638
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant
Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang
Tensile Strength, Yield 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali