| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | LG Chemical |
| Trade Name | LUMID |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
| Water Absorption | 0.60 % <br>@Temperature 23.0 °C,<br> Time 86400 sec |
0.60 % <br>@Temperature 73.4 °F,<br> Time 24.0 hour |
ASTM D570 |
| Maximum Moisture Content | 0.090 | 0.090 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.010 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.010 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 147 MPa <br>@Thickness 3.20 mm |
21300 psi <br>@Thickness 0.126 in |
5mm/min; ASTM D638 |
| Elongation at Break | 2.0 % <br>@Thickness 3.20 mm |
2.0 % <br>@Thickness 0.126 in |
5mm/min; ASTM D638 |
| Flexural Yield Strength | 216 MPa <br>@Thickness 3.20 mm |
31300 psi <br>@Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Flexural Modulus | 8.34 GPa <br>@Thickness 3.20 mm |
1210 ksi <br>@Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Izod Impact, Notched | 0.883 J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
1.65 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
| Melting Point | 260 °C | 500 °F | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C <br>@Thickness 6.40 mm |
491 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 248 °C <br>@Thickness 6.40 mm |
478 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 120 °C <br>@Thickness >=0.750 mm |
248 °F <br>@Thickness >=0.0295 in |
|
| 120 °C <br>@Thickness >=1.50 mm |
248 °F <br>@Thickness >=0.0591 in |
||
| 120 °C <br>@Thickness >=3.00 mm |
248 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 100 °C <br>@Thickness >=0.750 mm |
212 °F <br>@Thickness >=0.0295 in |
|
| 110 °C <br>@Thickness >=1.50 mm |
230 °F <br>@Thickness >=0.0591 in |
||
| 110 °C <br>@Thickness >=3.00 mm |
230 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 100 °C <br>@Thickness >=0.750 mm |
212 °F <br>@Thickness >=0.0295 in |
|
| 110 °C <br>@Thickness >=1.50 mm |
230 °F <br>@Thickness >=0.0591 in |
||
| 110 °C <br>@Thickness >=3.00 mm |
230 °F <br>@Thickness >=0.118 in |
||
| Flammability, UL94 | V-0 <br>@Thickness >=0.750 mm |
V-0 <br>@Thickness >=0.0295 in |
|
| V-0 <br>@Thickness >=1.50 mm |
V-0 <br>@Thickness >=0.0591 in |
||
| V-0 <br>@Thickness >=3.00 mm |
V-0 <br>@Thickness >=0.118 in |
||
| Glow Wire Test | 775 °C <br>@Thickness 0.800 mm |
1430 °F <br>@Thickness 0.0315 in |
IEC 60695-2-13 |
| 775 °C <br>@Thickness 1.60 mm |
1430 °F <br>@Thickness 0.0630 in |
IEC 60695-2-13 | |
| 775 °C <br>@Thickness 3.20 mm |
1430 °F <br>@Thickness 0.126 in |
IEC 60695-2-13 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.0 <br>@Frequency 1.00e+6 Hz |
3.0 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 22.0 kV/mm <br>@Thickness 1.00 mm |
559 kV/in <br>@Thickness 0.0394 in |
ASTM D149 |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
| Comparative Tracking Index | 400 V | 400 V | Solution A; IEC 60112 |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 265 - 275 °C | 509 - 527 °F | Injection Molding |
| Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
| Front Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
| Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
| Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |