Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 1430 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
PolyOne Bergamid™ A70 G25 U-SO TM Polyamide 66 (Nylon 66)
Information provided by PolyOne
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Glow Wire Test 775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
Glow Wire Test 775 °C

@Thickness 3.20 mm
1430 °F

@Thickness 0.126 in
IEC 60695-2-13
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
Glow Wire Test 775 °C

@Diameter 0.400 mm
1430 °F

@Diameter 0.0157 in
GWIT; IEC 60695-2-13
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant
PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS.
Glow Wire Test 775 °C

@Diameter 1.50 mm
1430 °F

@Diameter 0.0591 in
GWIT; IEC 60695-2-13
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant
PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS.
Glow Wire Test 775 °C

@Diameter 0.800 mm
1430 °F

@Diameter 0.0315 in
GWIT; IEC 60695-2-13
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS.
Glow Wire Test 775 °C

@Thickness 2.00 mm
1430 °F

@Thickness 0.0787 in
GWIT
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Glow Wire Test 775 °C

@Thickness 1.00 mm
1430 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Glow Wire Test 775 °C

@Thickness 1.00 mm
1430 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
Glow Wire Test 775 °C

@Thickness 1.00 mm
1430 °F

@Thickness 0.0394 in
GWIT
LATI Laticonther 83 CP/80 PA12, Impact Modified
High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Glow Wire Test 775 °C

@Thickness 1.00 mm
1430 °F

@Thickness 0.0394 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Glow Wire Test 775 °C

@Thickness 2.00 mm
1430 °F

@Thickness 0.0787 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East)
Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Glow Wire Test 775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Asia Pacific)
LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi..
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Glow Wire Test 775 °C

@Thickness 1.60 mm
1430 °F

@Thickness 0.0630 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Akulon® XG-FKGS6 PA6-GF30 FR
30% Glass Reinforced, Flame Retardant, Halogen free
Glow Wire Test 775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
Glow Wire Test 775 °C

@Thickness 0.800 mm
1430 °F

@Thickness 0.0315 in
ALL, Glow-Wire Ignition; IEC 60695-2-13
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Glow Wire Test 775 °C

@Thickness 0.800 mm
1430 °F

@Thickness 0.0315 in
Glow-Wire Ignition; IEC 60695-2-13
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded
Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym..
Glow Wire Test 775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Glow Wire Test 775 °C

@Thickness 0.750 mm
1430 °F

@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Glow Wire Test 775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
Ignition Temp; IEC 60695-2-12
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Glow Wire Test 775 °C

@Thickness 2.00 mm
1430 °F

@Thickness 0.0787 in
GWIT
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
IEC 60695-2-12
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Glow Wire Test 775 °C

@Thickness 0.900 mm
1430 °F

@Thickness 0.0354 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature condi..
Glow Wire Test 775 °C

@Thickness 0.900 mm
1430 °F

@Thickness 0.0354 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions...
Glow Wire Test 775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® MX 1004 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Copyright © lookpolymers.com All Rights Reserved