Polymer Property : Dielectric Strength = 22.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 22.0 kV/mm
559 kV/in
Pyrotek TS-110 Thermoset Electrical Insulation Product (Nema Grade: G-10)
Glass reinforcement, Epoxy Resin, Natural Color. High flexural, impact and bond strength at room temperature.Information provided by Pyrotek.
Dielectric Strength 22.0 kV/mm
559 kV/in
Quadrant EPP Ertalyte® PET, cast (ISO Data)
The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear.
Dielectric Strength 22.0 kV/mm
559 kV/in
dry; IEC 60243-1
Murtfeldt Murylat® Polyethylene Terephthalate
Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an..
Dielectric Strength 22.0 kV/mm

@Thickness 2.00 mm
559 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Dielectric Strength 22.0 kV/mm

@Thickness 2.50 mm
559 kV/in

@Thickness 0.0984 in
IEC 60243-1
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
Dielectric Strength 22.0 kV/mm
559 kV/in
1.6mm; ASTM D149
Kingfa JH720 G50 50% Glass Fiber Reinforced PC
Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p..
Dielectric Strength 22.0 kV/mm

@Thickness 1.00 mm
559 kV/in

@Thickness 0.0394 in
ASTM D149
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy
Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical
Dielectric Strength 22.0 kV/mm

@Thickness 1.00 mm
559 kV/in

@Thickness 0.0394 in
ASTM D149
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose
Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Dielectric Strength 22.0 kV/mm

@Thickness 1.00 mm
559 kV/in

@Thickness 0.0394 in
ASTM D149
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose
Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
Dielectric Strength 22.0 kV/mm
559 kV/in
Momentive Performance Materials TSE397 One Component RTV Adhesive Sealant/Coating, Clear/White
TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials i..
Dielectric Strength 22.0 kV/mm

@Thickness 1.59 mm
559 kV/in

@Thickness 0.0625 in
Perpendicular, Short Time in Oil and Air; ASTM D149
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2)
A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, ..
Dielectric Strength 22.0 kV/mm
560 kV/in
Perpendicular, short time in air; ASTM D149
Haysite H515 Polyester, High Temp Flex
H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t..
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Noryl RF1132 PPE+PP
PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned
Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr..
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
Dielectric Strength 22.0 kV/mm
559 kV/in
60Hz, Short Time, dry; ASTM D149
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B..
Dielectric Strength >= 22.0 kV/mm
>= 559 kV/in
IEC 60243
Borealis Visico™/Visico™ ME4425/LE4438 Polyethylene
Visico™ ME4425 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ ME4425 and Visico™ LE4438 is a combination of a Visico™ bas..
Dielectric Strength 22.0 kV/mm
559 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® TSGZ-50 PA666-GF50
Information provided by EMS Grivory
Dielectric Strength 22.0 kV/mm
559 kV/in
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..
Dielectric Strength 22.0 kV/mm
559 kV/in
ISO data
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi..
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149/DIN 53481
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric..
Dielectric Strength 22.0 kV/mm
559 kV/in
in transformer oil; IEC 60243-1
CENTROPLAST CENTROLYTE Polyethylene terephthalate
This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance. Applications include pump components, coil bodies, ball bearing cups and prote..