Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
|
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 0.810 mm |
230 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 0.810 mm |
230 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 0.750 mm |
230 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 0.750 mm |
230 °F @Thickness 0.0295 in |
UL 746B |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 0.750 mm |
230 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |