| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | ISO 75/2Bf |
|
Radici Radilon® ARV300 RKC (dry) Nylon 66
Glass-fiber reinforced with heat and hydrolysis resistanceInformation provided by Radici group.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | ISO 75B |
|
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
(discontinued **)
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
255
°C <br>@Thickness 6.40 mm
|
491
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Kingfa PA66-RG201 Flame Retardant, 20% Glass Fiber Reinforced PA66
Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation Provided by Kingf..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
255
°C <br>@Thickness 6.40 mm
|
491
°F <br>@Thickness 0.252 in
|
Unannealed; ASTM D648 |
|
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | |
|
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
255
°C <br>@Thickness 3.20 mm
|
491
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66
LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP LUBRICOMP RX94033 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RX94033 is a compound based on PA 66 resin containing Aramide Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | HDT B; Unannealed; ISO 75-2/B |
|
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 G/CF30 L BK 30% GlassCarbon Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF/M30 HS BK 10/20% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral Filler, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF/M38 HS BK 38% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 38% Filler by Weight and Mineral Filler, 38% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabili..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF14 HS L BK 14% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF15 TL5 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: PTFE Lubricant (5%)Features: LubricatedAppearance: Natural ColorInformation p..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF20 L 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF25 HS L 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedProcessin..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF33 5105 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GF5 L BK 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compos..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
255
°C <br>@Thickness 3.20 mm
|
491
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66
LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
255
°C <br>@Thickness 3.20 mm
|
491
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon
LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | DAM; ISO 75-1/-2 |
|
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | ISO 75 |
|
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | ISO 75 |
|
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural
Information provided by Eurotec®
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | ASTM D648 |
|
A. Schulman ComAlloy Hiloy® 621 Nylon 6/6, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | |
|
Radici Radilon® A RV330 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | |
|
Radici Radilon® A RV350 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | |
|
Radici Radilon® A RV500 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill® PA6/6 GFB20 20% Glass/Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabiliz..
|
|||