| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
|
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Average value: 79.9 °C Grade Count:5 |
|
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 7200 - 14400 sec
|
176
-
194
°F <br>@Time 2.00 - 4.00 hour
|
Pre-dry |
|
Kingfa H-12 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
|
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
|
LG Chemical KEYFLEX BT HB9255D Ester Type TPE
Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
|
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
|
|||
| Drying Temperature |
70.0
-
90.0
°C <br>@Time 10800 sec
|
158
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 12 (PA12) based compound. Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i..
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
|
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced
Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation ..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers. Good thermal propertiesAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North..
|
|||
| Drying Temperature |
70.0
-
90.0
°C <br>@Time 10800 sec
|
158
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Laticonther 83 CP/80 PA12, Impact Modified
High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latigray 52/11-01 CX/45 PP Homopolymer
Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
|
|||
| Drying Temperature | 85.0 - 90.0 °C | 185 - 194 °F | |
|
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
|
Diamond Polymers ABS 4011 HH
Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc.
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Pre-drying Temperature |
|
Asahi Kasei Xyron® 200H Modified Polyphenylene Ether
Heat ResistantInformation provided by Asahi Kasei
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
|
Asia International Enterprise (Hong Kong) 60G5 Nylon 66, 25% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Drying Temperature |
80.0
-
90.0
°C <br>@Time 10800 sec
|
176
-
194
°F <br>@Time 3.00 hour
|
|
|
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Extrusion Molding |
|
LG Chemical LI923 Extrusion ASA
Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Necessary, use a desiccant-type hopper dryer. |
|
LATI LARAMID G/30 30% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Necessary, use a desiccant-type hopper dryer. |
|
LATI LARAMID G/35 35% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
|
|||
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Necessary, use a desiccant-type hopper dryer. |
|
LATI LARAMID G/45 45% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Average value: 78.4 °C Grade Count:13 |
|
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..
|
|||