Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Keep the material always warm in a hopper at 70-80°C. Temperature can be reduced when using vacuum ovens. |
LATI LATAMID 12 H FE90 Nylon 12 Base Magnetizable Compound
(Unverified Data**) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Average value: 79.8 °C Grade Count:5 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Drying Temperature | 80.0 - 90.0 °C @Time 7200 - 14400 sec |
176 - 194 °F @Time 2.00 - 4.00 hour |
Pre-dry |
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,.. |
|||
Drying Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Injection Molding |
LG Chemical KEYFLEX TO1065A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Drying Temperature | 80.0 - 90.0 °C @Time 7200 - 18000 sec |
176 - 194 °F @Time 2.00 - 5.00 hour |
|
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Drying Temperature | 70.0 - 90.0 °C @Time 10800 sec |
158 - 194 °F @Time 3.00 hour |
|
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm.. |
|||
Drying Temperature | 70.0 - 90.0 °C @Time 10800 sec |
158 - 194 °F @Time 3.00 hour |
|
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Drying Temperature | 80.0 - 90.0 °C @Time 10800 sec |
176 - 194 °F @Time 3.00 hour |
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Drying Temperature | 80.0 - 90.0 °C @Time 10800 sec |
176 - 194 °F @Time 3.00 hour |
|
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Drying Temperature | 80.0 - 90.0 °C @Time 10800 sec |
176 - 194 °F @Time 3.00 hour |
|
LATI Latistat 52/7-02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Styron EMERGEâ„¢ 5100 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5100 is a pre-colored, white, ABS resin, having high opacity and excellent toughness intended for manufacture of laser-marketable injection-molded smart cards.Information provided b.. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
Diamond Polymers ABS 4011 HH Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Pre-drying Temperature |
Asahi Kasei Xyron® 240V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Drying Temperature | 80.0 - 90.0 °C @Thickness 30.0 mm |
176 - 194 °F @Thickness 1.18 in |
|
Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade Middle impact, Good mechanical strength, High flexural strengthInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Must be dried. Typical condition. |
BASF Elastollan® 690A15N Polyester Type Polyurethane Elastomer This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes.. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Must be dried. Typical condition. |
BASF Elastollan® M88A15 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Must be dried. Typical condition. |
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Drying Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Injection Molding |
LG Chemical KEYFLEX TO1075AR Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |