Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Mold Temperature | 50.0 - 104 °C | 122 - 220 °F | Average value: 79.5 °C Grade Count:29 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Mold Temperature | 50.0 - 60.0 °C | 122 - 140 °F | |
M. Holland Company MAGMA® LM372-A LLDPE
(discontinued **) Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 50.0 - 110 °C | 122 - 230 °F | Average value: 78.0 °C Grade Count:8 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Start Point: 60°C |
Kingfa PBT-RG20 Flame Retardant, 20% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | |
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | Surface |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Mold Temperature | 50.0 - 60.0 °C | 122 - 140 °F | |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Start Point: 60°C |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced EMI shielding product based on ABS/PC Blend (ABS/PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Mold Temperature | 50.0 °C | 122 °F | |
Solvay TECHNYL® A 258 PA Black 2N PA66, DRY Description: Unreinforced and modified polyamide 66, UV and thermal stabilized with excellent impact resistance, for injection molding.Available in: Europe Product Applications: TECHNYL® A 258P1 .. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
CP-Polymer-Technik Wellamid® 6000 HWV0CP Nylon 6, Flame Protection, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
CP-Polymer-Technik Wellamid® 6600/42 HWCP Nylon 66, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FE310001 NC010 Nylon 612 Zytel® FE310001 NC010 is a high viscosity polyamide 612 resin that is suitable for extrusion applications, such as monofilaments and tubing.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Starflam PX06004 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
Asahi Kasei Xyron® 500Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Asia International Enterprise (Hong Kong) 60T4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Injection Molding |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
Asahi Kasei Xyron® 340V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Asia International Enterprise (Hong Kong) 60T6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Asia International Enterprise (Hong Kong) ST60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |