| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | DAM; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.013 cm/cm <br>@Thickness 2.00 mm |
0.013 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm <br>@Thickness 2.00 mm |
0.013 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 58.0 MPa <br>@Temperature 23.0 °C |
8410 psi <br>@Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Modulus | 2.25 GPa <br>@Temperature 23.0 °C |
326 ksi <br>@Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Modulus | 2.00 GPa <br>@Temperature 23.0 °C |
290 ksi <br>@Temperature 73.4 °F |
DAM; ISO 178 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² <br>@Temperature 23.0 °C |
2.38 ft-lb/in² <br>@Temperature 73.4 °F |
DAM; ISO 180/1A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | DAM; ASTM D3418 |
| Deflection Temperature at 1.8 MPa (264 psi) | 56.0 °C | 133 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | DAM; Extrusion |
| 235 °C | 455 °F | DAM; Optimum; Extrusion | |
| 250 °C | 482 °F | DAM; Optimum; Injection Molding | |
| 230 - 290 °C | 446 - 554 °F | DAM; Injection Molding | |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
| 80.0 °C | 176 °F | DAM; optimum; Injection Molding | |
| Drying Temperature | 80.0 °C | 176 °F | DAM; Extrusion |
| 80.0 °C | 176 °F | DAM; Injection Molding | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Injection Molding |
| 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion | |
| Moisture Content | <= 0.050 % | <= 0.050 % | DAM; Extrusion |
| <= 0.050 % | <= 0.050 % | DAM; Injection Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 612 | DAM |
| Material Status | Preliminary Data | DAM |
| Part Marking Code | >PA612< | ISO 11469; DAM |
| Processing Method | Extrusion | DAM |
| Product Category | Extrusion Resins | DAM |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA612 | ISO 1043; DAM |