Polymer Property : Nozzle Temperature = 446 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 230 °C
446 °F
Inchem Phenoxy PKFE
Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation.
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance
Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical
Nozzle Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Nozzle Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUMAX IN-5001 High Impact PBT
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose
Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose
Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Nozzle Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
Nozzle Temperature 230 - 260 °C
446 - 500 °F
Gromax 1172LL TPE
1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac..
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica..
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0
Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil..
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 230 °C
446 °F
Tipco Tipcofil® AU 027 - Unfilled Nylon-6 Compound, with High Heat Stability, for Injection Molding
Unreinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Nozzle Temperature 230 °C
446 °F
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Unitika A1030JR PA6, Dry
Information provided by Unitika Ltd.
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® 7233 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7233 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Nozzle Temperature 230 - 255 °C
446 - 491 °F
Injection Molding
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Nozzle Temperature 230 - 305 °C
446 - 581 °F
Average value: 279 °C Grade Count:10
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR404T ABS, Heat Resistance
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical..