| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
|
Samyang Triloy® 410N PC/PET alloy, Flame Retardant
(discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
|
|||
| Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
|
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
|
|||
| Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
|
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
|
|||
| Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
|
Lehmann & Voss LUVOCOM® 65-8452-2 PP-copolymer, with carbon fiber, aramid reinforcement, lubricant modified
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Information provided by..
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
|
LG Chemical KEYFLEX BT HB9242D Ester Type TPE
Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
|
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
|
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
|
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
|
LG Chemical LUMID GP1300AP PA6, Plasticized
Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical Lupox® GP1000W PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
|
|||
| Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
|
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 250 °C | 392 - 482 °F | Injection Molding |
|
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC
Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical XR409E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical XR440 ABS, Low Emission High Heat ABS
Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
|
Gromax PBT 1200-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
LG Chemical XR407E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by..
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
|
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
|
Samyang Triloy® 215 PC/ABS alloy
Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl ..
|
|||
| Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Unitika AX-1500W Conditioned
Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis..
|
|||
| Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
|
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Coating |
|
Arkema Group Pebax® MV 3000 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
|
|||
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Cast Film |
|
Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
|
|||
| Nozzle Temperature | 245 - 250 °C | 473 - 482 °F | |
|
Gromax PBT 1100-211MB
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||