Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 225 - 245 °C
437 - 473 °F
Injection Molding
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 225 - 245 °C
437 - 473 °F
Injection Molding
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Injection
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance
Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose
Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose
Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose
Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance
Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical
Nozzle Temperature 235 - 245 °C
455 - 473 °F
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Nozzle Temperature 235 - 245 °C
455 - 473 °F
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Nozzle Temperature 235 - 245 °C
455 - 473 °F
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Nozzle Temperature 235 - 245 °C
455 - 473 °F
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Nozzle Temperature 230 - 245 °C
446 - 473 °F
Injection Molding
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 240 - 245 °C
464 - 473 °F
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin
20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 240 - 245 °C
464 - 473 °F
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 240 - 245 °C
464 - 473 °F
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 240 - 245 °C
464 - 473 °F
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 210 - 245 °C
410 - 473 °F
Injection Molding
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Nozzle Temperature 210 - 245 °C
410 - 473 °F
Injection Molding
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Nozzle Temperature 240 - 245 °C
464 - 473 °F
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin
10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 240 - 245 °C
464 - 473 °F
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin
30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 220 - 245 °C
428 - 473 °F
Average value: 233 °C Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Nozzle Temperature 210 - 245 °C
410 - 473 °F
Injection Molding
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..