Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | |
Multibase TPSiV® 4000-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 98 AE Thermoplastic Polyurethane Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Nozzle Temperature | 180 - 195 °C | 356 - 383 °F | |
KEP Kepital® F30 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate.. |
|||
Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | Extrusion |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
Stellarchem MP-855WR TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 180 °C | 356 °F | |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Nozzle Temperature | >= 180 °C | >= 356 °F | Injection |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA) Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | Average value: 200 °C Grade Count:18 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Nozzle Temperature | 180 - 195 °C | 356 - 383 °F | |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |