Unitika TERRAMAC TE-2000 Polylactic Acid (PLA)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer Unitika
Trade Name TERRAMAC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika TERRAMAC TE-2000 Polylactic Acid (PLA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.0 MPa
9140 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Flexural Strength 106 MPa
15400 psi
ISO 178
Flexural Modulus 4.30 GPa
624 ksi
ISO 178
Charpy Impact, Notched 0.160 J/cm²
0.761 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
Maximum Service Temperature, Air 240 °C
464 °F
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C
136 °F
ISO 75
Processing Properties Metric English Comments
Rear Barrel Temperature 130 - 170 °C
266 - 338 °F
Middle Barrel Temperature 180 - 220 °C
356 - 428 °F
Front Barrel Temperature 180 - 220 °C
356 - 428 °F
Nozzle Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
actual surface temp
Back Pressure 0.490 - 1.47 MPa
71.1 - 213 psi
gage pressure
Descriptive Properties Value Comments
Appearance Transparent