| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | |
|
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA
NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Noltex Soarnol® D2908 Ethylene Vinyl Alcohol Copolymer
Ethylene content 29 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer
Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The ..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Average value: 205 °C Grade Count:4 |
|
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
|
|||
| Nozzle Temperature | 175 - 220 °C | 347 - 428 °F | Average value: 201 °C Grade Count:5 |
|
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer
Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical HIPS MI770 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1140D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
|
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Lehmann & Voss LUVOCOM® TPE-0900 VP Thermoplastic elastomer, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Lehmann & Voss LUVOCOM® TPE-7829 Thermoplastic elastomer, with PTFE
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical ALPHALAC SG970NSU HIPS
Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | |
|
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Nozzle Temperature | 185 - 220 °C | 365 - 428 °F | Injection |
|
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection |
|
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection |
|
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer
Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection |
|
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer
Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Nozzle Temperature | 175 - 220 °C | 347 - 428 °F | Average value: 205 °C Grade Count:6 |
|
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
|
|||