Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 260 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 2004 R Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Front Barrel Temperature 221 - 260 °C
430 - 500 °F
Multibase Multi-Pro® 4005 M Polypropylene
Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Front Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Front Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow
Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Front Barrel Temperature 243 - 260 °C
470 - 500 °F
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose
Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Front Barrel Temperature 243 - 260 °C
470 - 500 °F
Firestone CL200-001 Nylon 6
Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Front Barrel Temperature 243 - 260 °C
470 - 500 °F
Firestone CLM200-001 Nylon 6
Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Front Barrel Temperature 230 - 260 °C
446 - 500 °F
Start Point: 240°C
Kingfa MAC-751 HF PC/ABS Alloy
Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical ..
Front Barrel Temperature 250 - 260 °C
482 - 500 °F
Start Point: 250°C
Kingfa MAC-851 PC/ABS Alloy
Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical ..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Start Point: 250°C
Kingfa PBT-T15 15% Mineral Filled PBT
Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Front Barrel Temperature 245 - 260 °C
473 - 500 °F
Injection Molding
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Front Barrel Temperature 246 - 260 °C
475 - 500 °F
Injection Molding
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Front Barrel Temperature 243 - 260 °C
470 - 500 °F
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded
V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 230 - 260 °C
446 - 500 °F
Start Point: 240°C
Kingfa MAC-701 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p..
Front Barrel Temperature 245 - 260 °C
473 - 500 °F
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified
Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Solvay TECHNYL® A 402 Natural FA PA66, DRY
Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Teknor Apex Beetle® MDM54 Nylon 6, Non-halogenated, Mineral Reinforced
Notes: MDM54 is a UL recognized, V-2 rated halogen and phosphorus-free flam retarded, mineral filled injection molding grade of nylon 6, primarily intended for electrical applications; U.L. 94 V-2 a..
Front Barrel Temperature 241 - 260 °C
465 - 500 °F
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
Front Barrel Temperature 232 - 260 °C
450 - 500 °F
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Front Barrel Temperature 232 - 260 °C
450 - 500 °F
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose
Data provided by Clariant Masterbatches
Front Barrel Temperature 246 - 260 °C
475 - 500 °F
Calsak CS-72L General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Solvay TECHNYL® A 303 Natural FA PA66, DRY
Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe Product Applications: TECHNYL® A 303 Natural FA offers three main advantages: high impact resistanc..