Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas.. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP532-00 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Natural Applications: Interior trimCenter tail light bezelPackage trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Front Barrel Temperature | 221 - 238 °C | 430 - 460 °F | |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Front Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
CTC X-PRO TF 1020 GP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1020 GP is a 20% talc reinforced polypropylene homopolymer. It has applications in general purpose industrial, automotive, consumer, and construction.Data provided by Composite Technologies.. |
|||
Front Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
CTC X-PRO TF 2104 GP Recycled Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 2104 GP is a 20% talc reinforced polypropylene homopolymer made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden products.D.. |
|||
Front Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |