| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | |
|
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
|
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced
Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)&
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
|
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
|
|||
| Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
|
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler
(discontinued **)
Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **)
Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe..
|
|||
| Front Barrel Temperature | 260 - 310 °C | 500 - 590 °F | |
|
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer
Impact modified, flame retardantThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where l..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose
Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
|
|||
| Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
|
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6
Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
|
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applicat..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Front Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro..
|
|||
| Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
|
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
|
Tisan TISLAMID® 66 UNR Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
Wellman Wellamid® FRGF25-66-N Flame Retardant Nylon 66, Lubricated, 25% Glass Fiber
Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
|
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **)
Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008..
|
|||