Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Start Point: 275°C |
Kingfa JH720 G20 20% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | Start Point: 275°C |
Kingfa JH820 Modified PC Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac.. |
|||
Front Barrel Temperature | 240 - 290 °C | 464 - 554 °F | Start Point: 270°C |
Kingfa PC-S923 Modified PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 290 °C | 482 - 554 °F | |
LG Chemical LUPOY GP-5306F General Purpose PC/ABS Alloy, 30% Polymer Alloy, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Front Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay Technyl® A216V15 15% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin.. |
|||
Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | Zone 3 |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | Zone 3 |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |