Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 235 - 280 °C | 455 - 536 °F | Start Point: 260°C |
Kingfa PC-S809 Modified PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Middle Barrel Temperature | 235 - 280 °C | 455 - 536 °F | Start Point: 260°C |
Kingfa PC-S923 Modified PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 255 - 280 °C | 491 - 536 °F | Injection Molding |
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Middle Barrel Temperature | 255 - 280 °C | 491 - 536 °F | Injection Molding |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 255 - 280 °C | 491 - 536 °F | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Compression Zone |
Solvay Technyl® A218 Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
Teknor Apex Beetle® MDF2 Nylon 6, 30% Short Glass Fiber Reinforced, Dry Notes: MDF2 is a heat stabilized 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Features: Heat Stabilized; Good Surface Finish Processin.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 UNR Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Middle Barrel Temperature | 255 - 280 °C | 491 - 536 °F | Injection Molding |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |