Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate (PC)
Manufacturer LG Chemical
Trade Name LUPOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive front ends, cluster pad main panel (instrument panel), lower cluster pad main, console box, glove box cover, door, wheel cover and cap, defroster grill, back mirror housingElectrical and Electronic: Monitor housing, fax housing, notebook PC housing, cellular phone case, fax and copy machine frame, CD ROM drive tray and main frame, relay case, connector, switchIndustrial Parts and Household Appliance: Helmet, terminal box, electrical tool housing, industrial bobbin, distributing board box, power tool component, gears and cams, water meter housingInformation Provided by LG Chem
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 108 MPa
15700 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 157 MPa
22800 psi
ASTM D790
Flexural Modulus 6.86 GPa
995 ksi
ASTM D790
Izod Impact, Notched 0.980 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 230 - 270 °C
446 - 518 °F
Middle Barrel Temperature 240 - 280 °C
464 - 536 °F
Front Barrel Temperature 250 - 290 °C
482 - 554 °F
Nozzle Temperature 250 - 290 °C
482 - 554 °F
Melt Temperature 260 - 300 °C
500 - 572 °F
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Drying Temperature 70.0 - 100 °C
158 - 212 °F
Dry Time 3 - 5 hour
3 - 5 hour
Screw Speed 40 - 70 rpm
40 - 70 rpm
Users viewing this material also viewed the following: