Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP CX05031 PS (Europe-Africa-Middle East) LNP* Lubricomp* CX05031 is a compound based on Polystyrene resin containing Graphite, Silicone. Added features include; Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² - NB | 1.43 ft-lb/in² - NB | Average value: 32.8 kJ/m² Grade Count:28 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Izod Impact, Notched (ISO) | 3.00 - 60.0 kJ/m² @Temperature -40.0 - 0.000 °C |
1.43 - 28.6 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 10.7 kJ/m² Grade Count:54 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 6.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 2.86 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.50 kJ/m² Grade Count:2 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) EP-N31MA Polypropylene EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furnitu.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant... |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp MB006SU PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MB006SU is a compound based on Polypropylene resin containing Glass Bead. Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | Low Temp; ISO 180/1eA |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 K20 Nylon 6 High density and high modulusInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl A2 1 Flame Retardant Nylon 66 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.00 - 5.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 2.38 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.25 kJ/m² Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D.. |