Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc | DAM; ASTM D792 |
Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
Water Absorption | 0.95 % @Temperature 23.0 °C |
0.95 % @Temperature 73.4 °F |
Immersion 24h; DAM; ASTM D570 |
2.7 % @Temperature 23.0 °C |
2.7 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62, Similar to | |
8.5 % @Temperature 23.0 °C |
8.5 % @Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62, Similar to | |
9.0 % @Temperature 23.0 °C |
9.0 % @Temperature 73.4 °F |
Saturation; DAM; ASTM D570 | |
Linear Mold Shrinkage | 0.012 cm/cm @Thickness 3.20 mm |
0.012 in/in @Thickness 0.126 in |
Flow; DAM |
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 121 | 121 | DAM; ASTM D785 |
Tensile Strength | 41.4 MPa @Temperature 77.0 °C |
6000 psi @Temperature 171 °F |
50%RH; ASTM D638 |
48.3 MPa @Temperature 77.0 °C |
7010 psi @Temperature 171 °F |
DAM; ASTM D638 | |
62.0 MPa @Temperature 23.0 °C |
8990 psi @Temperature 73.4 °F |
50%RH; ASTM D638 | |
83.0 MPa @Temperature 23.0 °C |
12000 psi @Temperature 73.4 °F |
DAM; ASTM D638 | |
111 MPa @Temperature -40.0 °C |
16100 psi @Temperature -40.0 °F |
50%RH; ASTM D638 | |
114 MPa @Temperature -40.0 °C |
16500 psi @Temperature -40.0 °F |
DAM; ASTM D638 | |
Tensile Strength, Yield | 60.0 MPa @Temperature 23.0 °C |
8700 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
85.0 MPa @Temperature 23.0 °C |
12300 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
Elongation at Break | 10 % @Temperature -40.0 °C |
10 % @Temperature -40.0 °F |
50%RH; ASTM D638 |
10 % @Temperature -40.0 °C |
10 % @Temperature -40.0 °F |
DAM; ASTM D638 | |
24 % @Temperature 23.0 °C |
24 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 | |
>= 25 % @Temperature 23.0 °C |
>= 25 % @Temperature 73.4 °F |
DAM; ASTM D638 | |
30 % @Temperature 23.0 °C |
30 % @Temperature 73.4 °F |
DAM; ISO 527 | |
>= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; nominal; ISO 527 | |
>= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
>= 120 % @Temperature 23.0 °C |
>= 120 % @Temperature 73.4 °F |
50%RH; ASTM D638 | |
>= 120 % @Temperature 77.0 °C |
>= 120 % @Temperature 171 °F |
DAM; ASTM D638 | |
>= 200 % @Temperature 77.0 °C |
>= 200 % @Temperature 171 °F |
50%RH; ASTM D638 | |
Elongation at Yield | 25 % @Temperature 23.0 °C |
25 % @Temperature 73.4 °F |
50%RH; ISO 527 |
Tensile Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
3.20 GPa @Temperature 23.0 °C |
464 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
Flexural Modulus | 0.690 GPa @Temperature 77.0 °C |
100 ksi @Temperature 171 °F |
DAM; ASTM D790 |
0.690 GPa @Temperature 77.0 °C |
100 ksi @Temperature 171 °F |
50%RH; ASTM D790 | |
1.38 GPa @Temperature 23.0 °C |
200 ksi @Temperature 73.4 °F |
50%RH; ASTM D790 | |
2.83 GPa @Temperature 23.0 °C |
410 ksi @Temperature 73.4 °F |
DAM; ASTM D790 | |
3.93 GPa @Temperature -40.0 °C |
570 ksi @Temperature -40.0 °F |
50%RH; ASTM D790 | |
4.48 GPa @Temperature -40.0 °C |
650 ksi @Temperature -40.0 °F |
DAM; ASTM D790 | |
Shear Strength | 65.5 MPa @Temperature 23.0 °C |
9500 psi @Temperature 73.4 °F |
50%RH; ASTM D732 |
72.4 MPa @Temperature 23.0 °C |
10500 psi @Temperature 73.4 °F |
DAM; ASTM D732 | |
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
0.590 J/cm @Temperature -40.0 °C |
1.11 ft-lb/in @Temperature -40.0 °F |
50%RH; ASTM D256 | |
0.590 J/cm @Temperature -40.0 °C |
1.11 ft-lb/in @Temperature -40.0 °F |
DAM; ASTM D256 | |
0.640 J/cm @Temperature 77.0 °C |
1.20 ft-lb/in @Temperature 171 °F |
DAM; ASTM D256 | |
1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 | |
2.70 J/cm @Temperature 77.0 °C |
5.06 ft-lb/in @Temperature 171 °F |
50%RH; ASTM D256 | |
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
12.0 kJ/m² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA | |
Tensile Impact Strength | 340 kJ/m² @Temperature 23.0 °C |
162 ft-lb/in² @Temperature 73.4 °F |
DAM; Long specimen; ASTM D1822 |
920 kJ/m² @Temperature 23.0 °C |
438 ft-lb/in² @Temperature 73.4 °F |
50%RH; Long specimen; ASTM D1822 | |
Tensile Creep Modulus, 1 hour | 1340 MPa @Temperature 23.0 °C |
194000 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
Tensile Creep Modulus, 1000 hours | 600 MPa @Temperature 23.0 °C |
87000 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 23.0 °C |
1.00e+12 ohm-cm @Temperature 73.4 °F |
50%RH; ASTM D257 |
1.00e+14 ohm-cm @Temperature 23.0 °C |
1.00e+14 ohm-cm @Temperature 73.4 °F |
DAM; ASTM D257 | |
Dielectric Constant | 3.4 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
3.4 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
DAM; ASTM D150 |
3.6 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
3.6 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
DAM; IEC 60250 | |
3.7 @Frequency 100 Hz, Temperature 23.0 °C |
3.7 @Frequency 100 Hz, Temperature 73.4 °F |
DAM; ASTM D150 | |
3.7 @Frequency 1000 Hz, Temperature 23.0 °C |
3.7 @Frequency 1000 Hz, Temperature 73.4 °F |
DAM; ASTM D150 | |
3.7 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
3.7 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
50%RH; ASTM D150 | |
4.6 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
4.6 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
50%RH; IEC 60250 | |
5.4 @Frequency 1000 Hz, Temperature 23.0 °C |
5.4 @Frequency 1000 Hz, Temperature 73.4 °F |
50%RH; ASTM D150 | |
6.5 @Frequency 100 Hz, Temperature 23.0 °C |
6.5 @Frequency 100 Hz, Temperature 73.4 °F |
50%RH; ASTM D150 | |
Dissipation Factor | 0.010 @Frequency 100 Hz, Temperature 23.0 °C |
0.010 @Frequency 100 Hz, Temperature 73.4 °F |
DAM; ASTM D150 |