| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Addiplast Addinyl B2 K20 Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.10 g/cc | 0.0759 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 83 | 83 | Conditioned; ISO 868 |
| 86 | 86 | ISO 868 | |
| Tensile Strength at Break | 24.0 MPa | 3480 psi | Conditioned; ISO R 527 |
| 33.0 MPa | 4790 psi | ISO R 527 | |
| Elongation at Yield | 10 % | 10 % | ISO R 527 |
| 40 % | 40 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 2.20 GPa | 319 ksi | Conditioned; ISO 178 |
| 5.00 GPa | 725 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | ISO 180/1A |
| 4.00 kJ/m² | 1.90 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179/IeU |
| NB | NB | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/IeA |
| 0.300 J/cm² | 1.43 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.0 °C | 162 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 475 V | 475 V | CEI 60112/Solution A |