Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | SABIC Method |
SABIC Innovative Plastics LNP COLORCOMP J1000Z PES (Europe-Africa-Middle East) LNP* COLORCOMP* is a compound based on Polyethersulfone resin. Added features include: High Viscosity |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | |
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.017 cm/cm | 0.010 - 0.017 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® TPX-HTN-000BB Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Time 86400 sec |
0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific) LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Time 86400 sec |
0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.00 mm |
0.010 in/in @Thickness 0.118 in |
|
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.00 mm |
0.010 in/in @Thickness 0.118 in |
|
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT13-66 XE-NBK1 13% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | MD |
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | Sim. To ISO 294-4 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm @Thickness 4.00 mm |
0.010 - 0.015 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide R1000IX2 PA66, Impact Modified, Injection Molded Staramide R1000IX2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as Star X 1010)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | |
BASF Procom® D 1012 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | Sheet |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Linear Mold Shrinkage, Flow | 0.010 cm/cm | 0.010 in/in | ISO 294-4,2577 |
Suzhou Hipro Polymers Hiprolon® 90 MC HLS G30 Nylon 612, 30% glass fiber filled Hiprolon® 90 MC HLS G30 is a polyamide 6.12 compound reinforced with 30% chopped glass fiber, and is used for injection molding. Features: high dimension stability, chemical resistance, impact resi.. |