Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Laticonther 52/35 CP1/45 PP Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LATI
Trade Name Laticonther
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Laticonther 52/35 CP1/45 PP Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Linear Mold Shrinkage, Flow 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.0 MPa
3190 psi
Elongation at Break 1.2 %
1.2 %
Tensile Modulus 3.40 GPa
493 ksi
Charpy Impact Unnotched 0.500 J/cm²
2.38 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 3.50 W/m-K
24.3 BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: