Techmer ES Plastiblend® TPX-HTN-000BB

Category Polymer , Thermoplastic , Nylon , High Temperature Nylon
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® TPX-HTN-000BB.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Water Absorption 1.8 %

@Time 86400 sec
1.8 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 100 MPa
14500 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 2.65 GPa
385 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.2 µm/m-°C
39.0 µin/in-°F
ASTM D696
Melting Point 110 °C
230 °F
Maximum Service Temperature, Inert 133 °C
272 °F
ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Unannealed; ASTM D648