Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | Euronil |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | ASTM D955 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0050 cm/cm | 0.0035 - 0.0050 in/in | |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latamid SP2 H2 G/35 PA 6.12, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latilub 82-05GR G/30 PA12, 30% Glass Fiber Reinforced, Graphite Filled Self-lubricating product based on Polyamide 12 (PA12). Graphite. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0050 cm/cm | 0.0035 - 0.0050 in/in | |
LATI Latiohm 66-05 PD01 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0050 cm/cm | 0.0035 - 0.0050 in/in | |
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | |
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0035 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | Rhodia Test |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.00 mm |
0.0035 in/in @Thickness 0.118 in |
|
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0075 cm/cm | 0.0035 - 0.0075 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF1583-WT1 44% Mineral/Glass Reinforced Nylon 6 Description: Mineral/Glass Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | DAM; 60x60x2mm; ISO 294-4 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latimass 82-05 D040 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |