Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 500 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP DFL24 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL24 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
PolyOne Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 2.00 mm |
0.0020 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | |
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | |
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ G1500A-M61 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. Main Features:High strengthHeat resistanceExamples of applications:Structural partsSteel alternating parts |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | |
LATI Latilub 87/28-17ST K/15 PC, 15% Carbon Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polycarbonate (PC). Silicone / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM AR9300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics ULTEM PW2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Time 86400 sec |
0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC (Asia Pacific) LNP* Thermocomp* DX06412H is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66 LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PES GM20 WT139 20% Milled Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp ZF0041XC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF0041XC is a compound based on PPE+PS Blend resin containing Glass Fiber and Flame retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Euro.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | DAM; ISO 294-4 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; E2P method |
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | on Tensile Bar; E2P method |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Thickness 4.00 mm |
0.0020 - 0.0050 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Eurotec |
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Sorona® 2045G BK346A Polytrimethylene Terephthalate (PTT)
(Unverified Data**) 45% Glass Reinforced Polytrimethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Sheet |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |